Submicron violet tungsten oxide may be used to prepare submicron tungsten powder (W powder). Cyclic Oxidation-reduction Method to Produce Submicron Tungsten Powder Step one: First reduction of violet tungsten oxide in hydrogen (H2), when temperature reached 860°C, keep it warm for 20min. Step two: Use tungsten powder obtained in step one, slowly heat it to 500°C in air, process the first oxidation when temperature reaches 500°C, and then keep it warm for 10min. Step three: Use sample of step two…